So I recently stripped 3 Space Marines and came out with them stripped of all the paint, but still with a heavy staining of primer. I then proceeded to re-spray said mini's using Halfords Grey Primer on a moderately warm day at a range of around 30cm from the model, in short sweeping passes. Now, from the method I've described, I can't see for the life of me how I've done it wrong - it's the method I always follow with good results. However, I've been left with 3 mini's with a very rough, pitted surface. I've put on a base coat and tested out a main coat on one of the Space Marines but I'm unsatisfied with the result as the pitting is very evident - is there any way I can rectify this situation, or am I best just binning the marines?
|